1) What is the process of increasing carbon percentage on the surface of low carbon steel?
Hardening
Nitriding
Carburizing
Tempering
Show Answer
Report Question
What's wrong with this question?
Report
Correct Answer: Carburizing
Question Details
1) What is the process of increasing carbon percentage on the surface of low carbon steel?
Hardening
Nitriding
Carburizing
Tempering
2) What is the preheating temperature of steel?
Upto 400 Degree Centigrade
Upto 500 Degree Centigrade
Upto 600 Degree Centigrade
Upto 300 Degree Centigrade
Show Answer
Report Question
What's wrong with this question?
Report
Correct Answer: Upto 600 Degree Centigrade
Question Details
2) What is the preheating temperature of steel?
Upto 400 Degree Centigrade
Upto 500 Degree Centigrade
Upto 600 Degree Centigrade
Upto 300 Degree Centigrade
3) Which gas is used in nitriding process?
Ammonia
Helium
Carbon dioxide
Hydrogen
Show Answer
Report Question
What's wrong with this question?
Report
Correct Answer: Ammonia
Question Details
3) Which gas is used in nitriding process?
Ammonia
Helium
Carbon dioxide
Hydrogen
4) What is the heating temperature in gas nitriding process?
Up 200 Degree Celsius
Up 300 Degree Celsius
Up 400 Degree Celsius
Up 500 Degree Celsius
Show Answer
Report Question
What's wrong with this question?
Report
Correct Answer: Up 500 Degree Celsius
Question Details
4) What is the heating temperature in gas nitriding process?
Up 200 Degree Celsius
Up 300 Degree Celsius
Up 400 Degree Celsius
Up 500 Degree Celsius
5) How many fundamental deviations are recommended by BIS?
25
24
20
30
Show Answer
Report Question
What's wrong with this question?
Report
Correct Answer: 25
Question Details
5) How many fundamental deviations are recommended by BIS?
25
24
20
30